Product Display
  • Flexibilizer
    PC Flexibilizer
    PS Flexibilizer
    PP Flexibilizer
    PE Flexibilizer
    PA Flexibilizer
    PET Flexibilizer
    PBT Flexibilizer
    POE Flexiblizer
    ABS Flexibilizer
    HIPS Flexibilizer
  • Color Masterbatch
    Black Masterbatch
    White Masterbatch
    Other Color Masterbatch
    Titanium white powder
  • Filling Masterbatch
    Caco3 Masterbatch
    Carbonate masterbatch
    Barium carbonate masterbatch
    ABS Special Caco3 Masterbatch
    Transparent Filling masterbatch
    Talcum powder
  • Other Functional Modifier Masterbatch
    Brightener agent
    Opening agent
    Electrostatic agent
PC/ABS alloy material should be dried before processing
1
Issuing time:2018-06-06 10:08

PC/ABS alloy material should be dried before processing


PC/ABS alloy is a kind of excellent engineering plastics. It is the blending and extrusion of PC and ABS to make PC/ABS alloy, which can synthesize the excellent properties of both. On the one hand, it can improve the heat resistance and tensile strength of ABS. On the other hand, it can reduce the viscosity of the melt of PC, improve the processing performance, reduce the sensitivity of the corresponding force and reduce the sensitivity of the corresponding force. Low cost. Therefore, PC/ABS alloy materials have been widely used in automobile, machinery, household appliances, computers, communication tools, office equipment and other industries.

PC/ABS alloy material can be injected or extruded and processed two times by traditional processing equipment, and injection molding is the most widely used. Due to the content of PC components and flame retardant, the small amount of water in PC/ABS alloy can easily lead to the hydrolysis of PC during the process of high temperature molding, and the partial degradation and small molecular precipitation caused by excessive heating, resulting in the appearance and strength problems of silver silk, yellow, color difference, product crisp and spray cracking. To control the relevant links.

PC/ABS alloy material will absorb moisture in air, with water content between 0.2~0.3%. In order to make the best effect of the injection products and reduce the possibility of degradation, the PC/ABS must be dried before the molding process, so that the water content of the material is reduced to less than 0.04%, and it is better to be below 0.02% to improve the processing stability and mechanical properties.

Normally, the PC/ABS alloy material is pre dried at 4~6 temperature for the recommended temperature, and the required moisture content can be achieved. The drying time is related to the drying equipment, but the longest cumulative drying time can not exceed 48 hours, otherwise the material may have the possibility of degradation and discoloration. There are three commonly used drying equipment: box dryer, hopper dryer and dehumidifier dryer. PC/ABS alloy material recommends dehumidification dryer to dry


All comments(0)
Pro ~ come to comment Oh!
Shenzhen Kadide Plastics Products Co.,Ltd

        Company address: No. 102, M16 building, Hua Nan Cheng chemical industry zone, Pinghu Town, Shenzhen.
            Factory address: Zhangmu Shenzhen Zhangyang Plastic Industrial Park Technology Park.Dongguan

                                              Tel:0755-89630482
                                             Fax:0755-89630483
                                          Email:Sales@kadideplastics.com
                                      Website:www.kadideplastics.com
qrCode
扫描查看手机版网站
Login
Login
Login by:
My Profile
leave a message
back to the top